France AFNOR AIR 9160 C, Z100CD17 Specialsteel AIR 9160 Z100CD17 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | Z100CD17 | AFNOR | France | AIR 9160 Z100CD17 |
Chemical composition(mass fraction)(wt.%) of the Z100CD17
C | Si | Mn | P | S | Cr | Ni | Mo |
---|---|---|---|---|---|---|---|
0.95 -1.10 | ≤1.00 | ≤1.00 | ≤0.030 | ≤0.020 | 16.0 -18.0 | ≤0.75 | 0.35 -0.75 |
Mechanical Properties of steel grade Z100CD17
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
156 (≥) | 645 (≥) | 11 | 32 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 |
Physical Properties of steel grade Z100CD17
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
44 | – | – | 0.34 | – | |||
916 | 536 | – | 31.3 | 341 | – | ||
936 | – | 13 | 44.2 | 323 | 411 |
Heat Treatment of steel grade Z100CD17
Heat treated : 1631°C – 1728°C
Technological Curves of steel grade Z100CD17
No Curve
Cross Reference Table (Equivalent Grade) of Z100CD17
Grade | Standard | Country | Application |
---|---|---|---|
Z100CD17CI | |||