Zeron 100
Zeron 100 Chemical composition:
Cr | Ni | Mo | N | Cu | C | Si | Mn | S | P | |
Min | 24 | 6 | 3 | 0.2 | 0.5 | ≤ | ||||
Max | 26 | 8 | 4 | 0.3 | 1 | 0.03 | 1 | 1 | 0.02 | 0.035 |
Zeron 100 Physical properties:
Densityg/g·cm-3 | Specific heat capacity/J·(kg·K)-1 | Resistivity
/10-6Ω ·m |
Young’s modulus of elasticity/GPa |
7.84 | – | 0.85 | 19 |
Zeron 100 Mechanical properties:
Plate thickness/mm | db/MPa | do.2/MPa | δs/% | hardness(HRC) | Impact value (V-type)Akv/J | |
20℃ | -30℃ | |||||
10 | 874 | 671 | 734 | 42 | 241 | 207 |
12 | 865 | 690 | 737 | 38 | 227 | 227 |
19 | 843 | 647 | 701 | 40 | 211 | 183 |
34 | 853 | 627 | 700 | 32 | 241 | 248 |
Zeron 100 Alloy properties:
Like other super duplex stainless steels, the microstructure of this steel is also a duplex structure with a α/γ close to 1 under solution conditions, but there will also be intermetallic phases and nitride precipitation on the steel matrix during cooling from high temperature to room temperature, including incorrect heat working, heat treatment and welding processes.
Zeron 100 Uses of alloys:
Zeron 100 is mainly used for offshore oil and gas exploitation, in the power station flue gas desulfurization, petrochemical engineering and fertilizer industry, the manufacture of reactors, containers, various heat exchangers, pipelines, pumps, valves, etc.
Zeron 100 Process performance:
Soldering process: Soldering is performed using SMAW, GTAW and SAW methods.
Heat treatment: Zeron 100 suitable heat treatment temperature is 1000~1100 °C, fast cooling after heat preservation.
Relevant standards: