HuaNickel X6CrNiTi18-10 stainless steel is a titanium stable grade that is typically used in the 1000-1600°F temperature range. For operating temperatures up to 1600°F, a stable treatment of 1550-1650°F, air cooling, can be used to provide optimal resistance to intergranular corrosion and polysulfuric acid stress corrosion cracking. X6CrNiTi18-10 stainless steel is easily welded by all common methods, including water arcing. The appropriate weld fillers are AWS ER347 bare wire and E347 overlay electrodes. The machinability of HuaNickel X6CrNiTi18-10 stainless steel is similar to that of 304 stainless steel. Compared to AISI B1112, it has a machinability rate of 45%.

X6CrNiTi18-10Chemical composition:

  Cr Ni Mo Ti C Mn Si P N Fe
Min 17 9 5x(C+N) 0.25 Bal
Max 19 12 0.75 0.7 0.08 2 1 0.045 0.1

X6CrNiTi18-10Physical properties:

Density Melting point
0.286 lb/in³ 2550 – 2600°F

X6CrNiTi18-10Mechanical properties:

Average high-temperature tensile properties

Temperature, °F 68 400 800 1000 1200 1350 1500
Ultimate tensile strength, ksi 93.3 73.6 69.5 63.5 52.3 39.3 26.4
0.2% yield strength, ksi 36.5 36.6 29.7 27.4 24.5 22.8 18.6

The average stress at break

Temperature,°F 1050 1100 1150 1200 1250 1300 1350 1400 1450 1500
1000hour,ksi 34 29 22 17.5 13 11.5 7.5 6.5 5 4
10000hour,ksi 27.5 22 16 12.5 9 7 5 4 3 2.5
100000hour,ksi 21.5 15 10.5 7.5 5 4 3.5 2.5 2.3 2

X6CrNiTi18-10Stainless steel characteristics:

Oxidation resistance 1600°F

Prevents intergranular corrosion in the weld heat-affected zone (HAZ).

Resistant to polysulfuric acid stress corrosion cracking

X6CrNiTi18-10Uses of stainless steel:

Aircraft piston engine manifolds

Expansion joints, thermal oxidants

Refinery equipment

High-temperature chemical process equipment

Relevant standards:

ASTM: A 240, A 276, A 312, A 479 GE: B50T1181

ASME: SA-240, SA-276, SA-312, SA-479