UNS S32205

Loader Loading...
EAD Logo Taking too long?

Reload Reload document
| Open Open in new tab

Download [1.39 MB]

HuaNickel UNS S32205 is an austenitic-ferritic duplex stainless steel with excellent corrosion resistance and strength characteristics. Compared with HuaNickel SUS 316L and SUS 317L, it has better local corrosion resistance and can be used in complete chemical equipment and seawater desalination equipment.

UNS S32205Chemical composition:

  C Si Mn P S Ni Cr Mo N
Min 4.5 22 3 0.14
Max 0.03 1 2 0.03 0.02 6.5 23 3.5 0.2

UNS S32205Physical properties:

Specific heat(J/kg・K) 460
Resistivity(μΩ・cm) 87.0
Thermal conductivity(W/m・K) 13.9
Average coefficient of thermal expansion(10-6/℃) 20–100℃ 12.7
20–200℃ 13.1
20–300℃ 13.5
20–400℃ 13.8
Longitudinal modulus of elasticity(MPa) 19.5 x  10^4
Ferromagnetic Yes
Melting point(℃) 1420-1465

UNS S32205Mechanical properties:

0.2%Yield strength
(N/mm2)
Tensile strength
(N/mm2)
Elongation
(%)
Hardness
≧ 450 ≧ 655 ≧ 25 (Hv) (HB)
93 455 572

UNS S32205Alloy properties:

Corrosion Resistance:

Steel Critical point corrosion temperature (℃) Critical crevice corrosion temperature (℃)
UNS S32205 50 25
SUS 316L 10 0℃hereinafter

UNS S32205Uses of alloys:

Typical applications include pumps, valves, flanges, and piping systems for a wide range of applications in the oil and gas, chemical, power, and brewing industries.

Contact

Detail datasheet