SUS 347

Loader Loading...
EAD Logo Taking too long?

Reload Reload document
| Open Open in new tab

Download [1.21 MB]

In a strong oxidizing environment, the corrosion resistance of TypeHuaNickel  SUS 347 stainless steel is slightly improved compared to Type 321 stainless steel. Type HuaNickel SUS 347 is stable with a column and is more suitable for aqueous and cryogenic environments due to its good resistance to intergranular attack. Both SUS 347 and 321 are resistant to good polysulfuric acid stress corrosion cracking.

SUS 347Chemical composition:

  Fe Cr Ni Cb+Ta C Si Mn P S
Min Bal 17 9 Cb 10xc (Cb 8xC) 0.04
Max 19 13 1 0.08 0.75 2 0.45 0.03

SUS 347Physical properties:

Density Melting point
0.282 lb/in3 2550 – 2635°F

SUS 347Mechanical properties:

Temperature, °F 68 400 800 1000 1200 1350 1500
Ultimate tensile strength, ksi 93.3 73.6 69.5 63.5 52.3 39.3 26.4
0.2% yield strength, ksi 36.5 36.6 29.7 27.4 24.5 22.8 18.6

SUS 347Stainless steel characteristics:

Good creep strength up to 1500°F

Maintains good corrosion resistance in applications with temperatures between 800°F and 1500°F

Under welding conditions, it has good resistance to intergranular corrosion

SUS 347Uses of stainless steel:

Refineries, Fluid Catalytic Cracking Units (Face-Centered Cubes), Booms, Recovery Tube Sheet Housings, Brackets,

Relevant standards:

AMS: 5512 ASTM: A 240, A 262 Practice E ASME: SA-240

PWA: F17 LCS, PWA 300 MSRR:5632