SUS 317L
Loading...
SUS 317LChemical composition:
Ni | Cr | Mo | Mn | Si | C | N | S | P | Fe | |
Min | 11 | 18 | 3 | – | – | – | – | – | – | Bal |
Max | 15 | 20 | 4 | 2 | 0.75 | 0.03 | 0.1 | 0.03 | 0.45 |
SUS 317LPhysical properties:
Density | Melting point | Poisson’s ratio | Resistivity |
0.285 lb/in3 | 2540 – 2630°F | 0.3 | 475 Ohm-circ mil/ft |
SUS 317LMechanical properties:
Ultimate tensile strength, ksi | 70 |
0.2% yield strength, ksi | 30 |
Elongation, % | 40 |
Hardness max., Brinell | 217 |
SUS 317LStainless steel characteristics:
Improved general and localized corrosion to 304/304L and 316/316L stainless steels
Good formability
Good weldability
SUS 317LUses of stainless steel:
FGD system、Chemical Process Containers、Petrochemical、Pulp、Power generation condensers
Relevant standards:
ASTM: A 240 ASME: SA-240