On the basis of 00Cr29Mo4TiNb steel, HuaNickel SEA-CURE is developed in order to improve the plasticity, toughness, weldability, thermal stability and hydrogen embrittlement resistance of the steel, reduce chromium and nickel and use Ti+Nb double stabilization. Together with the aforementioned Cr29Mo4 (Ti, Nb), SEA-CURE is also one of the most well-known super ferritic stainless steels currently used in the heat transfer tube of seawater condenser in power plants.

SEA-CUREChemical composition:

  Fe Cr Ni Mo Ti V B C AI Si Mn P S
Min Bal 13 24.5 1 2.4 0.01 0.005          
Max 16 28.5 1.75 3.2 0.1 0.025 0.06 0.35 0.35 0.75 0.025 0.025

SEA-CUREPhysical properties:

Density

p/g·cm~3

Linear expansion

coefficienta/10-6·K-1

Thermal conductivityA/W·(m·K)-1 Specific heat capacityc/J · (kg·K)-1
20~100℃ 20~150℃ 20~250 ℃ 20℃ 150℃ 200℃
7.8 9.68 9.77 10.66 15.9 19.5 20.6 500

SEA-CUREMechanical properties:

Temperature/℃ d,z/MPa σb/MPa δ/%
23 517 620 25
93 455 572 24
149 392 538 23
204 365 517 21
260 345 517 21

SEA-CUREAlloy properties:

The microstructure of this steel is the same as that of all super ferritic stainless steels, and the matrix structure of this steel has a body-centered cubic ferrite structure, and when heated at medium temperature (sensitized or welded heat-affected zone), there will be intermetallic compounds such as carbon, nitride and σ on the matrix, which will adversely affect the properties of the steel.

SEA-CUREUses of alloys:

This steel is mainly used for seawater corrosion-resistant pipelines, seawater condensers, heat exchangers, etc., and the price is far cheaper than copper, copper alloys and titanium.

SEA-CUREProcess performance:

Welding process: SEA-CURE steel has good welding performance. It can be welded by common welding methods of stainless steel, such as GTAW (with or without wire filling), GMAW, SMAW, etc.

Heat treatment: SEA-CURE is suitable for heat treatment at a temperature of 950~1100°C, and it is quickly cooled after heating and heat preservation.

Relevant standards:

ASTM A268/A268M-2020