NS341
NS341Chemical composition:
Ni | Cr | Mo | Cu | Ti | C | Fe | Si | Mn | P | S | |
\Min | Bal | 19 | 2 | 1 | 0.4 | ≤ | |||||
Max | 21 | 3 | 2 | 0.9 | 0.03 | 7 | 0.7 | 1 | 0.03 | 0.03 |
NS341Physical properties:
Density | 8.1g/cm³ |
Melting point | 1350~1390°C |
NS341Mechanical properties:
Solution treatment temperature/℃ | tensile strengthσb/Mpa≥ | Yield strength | Elongation |
1050~1100 | ≥ | ||
590 | 195 | 40 |
NS341Alloy properties:
NS341 alloy is resistant to a variety of acidic media, including strong acids such as nitric acid and sulfuric acid, as well as certain organic acids; NS341 alloy can still maintain its corrosion resistance and mechanical properties at high temperatures, which is suitable for applications in high temperature environments; HuaNickel NS341 alloy has good machinability
NS341Uses of alloys:
It is used in chemical equipment, oil and gas industry, power industry, aerospace, food processing, etc. Specific applications include heat treatment furnaces, exhaust systems, heat exchangers, pressure vessels, pipes, flanges, etc.
NS341Process performance:
Welding performance: NS341 alloy has good welding performance, and a variety of welding methods can be used, such as TIG welding, MIG welding, arc welding, etc.
Heat treatment: The annealing temperature is usually between 9801040°C, and the holding time depends on the thickness and size of the material; Solution treatment is to heat NS341 alloy to a higher temperature (about 11001150°C) for a certain period of time
Relevant standards:GB/T 15008-2020