NS1102
H08810Chemical composition:
C | Cr | Ni | Ti | AI | Fe | Mn | Si | P | S | Cu | |
Min | 0.05 | 19 | 30 | 0.15 | 0.15 | 38 | ≤ | ||||
Max | 0.1 | 23 | 35 | 0.6 | 0.6 | 47 | 0.15 | 1 | 0.03 | 0.015 | 0.75 |
H08810Physical properties:
Density | 8.0g/cm3 |
Melting point | 1350-1400℃ |
H08810Mechanical properties:
tensile strengthRm N/mm2 | Yield strengthRP0.2N/mm2 | ElongationA5 % |
450 | 180 | 35 |
H08810Alloy properties:
Excellent corrosion resistance in aqueous media at very high temperatures up to 500°C; Very good resistance to stress corrosion; Very good processability.
H08810Uses of alloys:
It is widely used in chemical, petroleum, pharmaceutical and sewage treatment fields.
H08810Process performance:
Welding process: HuaNickel H08810 can be welded by common welding methods, such as argon arc welding (TIG), arc welding (MIG), etc.
Heat treatment:
Solution treatment: Solution treatment is mainly used to dissolve alloying elements into the matrix, improve the uniformity of the alloy, and prepare for subsequent aging treatment. Aging treatment: Through aging treatment, the precipitated phase in the alloy is refined and evenly distributed, thereby improving the strength and hardness of the alloy.
Relevant standards:GB /T 15007-2017