Nitronic50
Loading...
Nitronic50Chemical composition:
Ni | Cr | Mo | Mn | Si | C | N | S | P | Cb | V | Fe | |
Min | 11.5 | 20.5 | 1.5 | 4 | – | – | 0.2 | – | – | 0.1 | 0.1 | Bal |
Max | 13.5 | 23.5 | 3 | 6 | 1 | 0.06 | 0.4 | 0.03 | 0.045 | 0.3 | 0.3 |
Nitronic50Physical properties:
Density | 0.285 lb/in3 |
Melting point | 2579 – 2642°F |
Resistivity | 492 ohm circ-mil/ft |
Nitronic50 Mechanical properties:
Temperature, °F | -320 | -100 | 75 | 200 | 400 | 600 | 800 | 1000 | 1200 | 1350 | 1500 |
Ultimate tensile strength, ksi | – | – | 117 | 107 | 96 | 92 | 89 | 84 | 74 | 66 | 52 |
0.2% yield strength, ksi | – | – | 60 | 50 | 38 | 35 | 34 | 32 | 31 | 31 | 30 |
Elongation, 2% | – | – | 45 | 43.5 | 43.5 | 42.5 | 43.5 | 41 | 38 | 37 | 41 |
Impact strength | 50 | 115 | 170 | – | – | – | – | – | – | – | – |
Nitronic50Stainless steel characteristics:
High-strength austenitic alloys
Good corrosion resistance
Nitronic50Uses of stainless steel:
Seawater pump shaft、heat exchanger、Pressure vessels、Marine hardware
Relevant standards:
ASTM: A 276 NACE: MR0175 ISO: 15156-3