NiCr33Mo8
NiCr33Mo8Chemical composition:
Ni | Cr | Mo | Fe | Si | Mn | Al | C | |
Min | Bal | 33 | 8 | ― | ― | ― | ― | ― |
Max | ― | ― | 2.0 | 0.6 | 0.5 | 0.4 | 0.05 |
NiCr33Mo8Physical properties:
Melting point/℃ | Density/g·cm-3 | Thermal conductivity/W·(m·℃)-1 | Linear expansion coefficient/×10-6℃-1 | |||||
Room temperature | 100℃ | 300℃ | 500℃ | 21~100℃ | 21~300℃ | 21~500℃ | ||
1332~1361 | 8.22 | 10 | 12 | 16 | 19 | 13.3 | 13.2 | 13.6 |
Specific heat capacity/J·(kg·℃)-1 | Resistivity/μΩ ·m | |||||||
Room temperature | 100℃ | 300℃ | 500℃ | Room temperature | 100℃ | 300℃ | 500℃ | |
450 | 470 | 510 | 530 | 1.18 | 1.19 | 1.21 | 1.24 |
NiCr33Mo8Mechanical properties:
Variety of materials | Solution treatment temperature℃ | Material size/mm | b/MPa | d0.z/MPa | δ/% |
sheet | 1135 | thick3.2 | 745 | 348 | 59 |
Medium and heavy plates | 112 | thick6.4 | 703 | 344 | 66 |
Medium and heavy plates | 1121 | thick12.7 | 689 | 318 | 72 |
Rods | 1121 | p1.0 | 710 | 319 | 66 |
Rods | 1121 | φ2.5 | 689 | 338 | 68 |
NiCr33Mo8Alloy properties:
Corrosion resistance: HuaNickel NiCr33Mo8 has excellent corrosion resistance, it is able to resist a variety of highly corrosive media such as nitric acid, chloride and other oxidizing acids. Corrosiveness: NiCr33Mo8 excels in a wide range of chloride-containing and oxidizing salt solutions, especially in low and medium temperature HCl environments.
High temperature strength: This alloy can still maintain high strength and hardness at high temperatures, and has good high temperature creep properties.
Antioxidant Properties: NiCr33Mo8 has significant antioxidant properties. This alloy can effectively resist the erosion of various oxidizing media in high temperature environments.
NiCr33Mo8Uses of alloys:
The alloy is mainly used in evaporators in the production of wet phosphoric acid, and in the pickling vessels of nitric acid and hydrofluoric acid solutions; equipment and components in corrosive environments of nitric acid and chloride in the chemical industry; caustic neutralization system devices and components that are resistant to high temperature (650°C) corrosion, etc.
NiCr33Mo8Process performance:
Welding process: HuaNickel NiCr33Mo8 weldability, commonly used welding processes include gas tungsten arc welding (GTAW) and gas metal arc welding
Thermal treatment: The heat treatment of NiCr33Mo8 mainly includes solution treatment and aging treatment. Solution treatment is a commonly used heat treatment that can significantly improve the properties of materials.
Relevant standards:
SB 575/B 575、SB 574/B 574 B 472 、SB 622/B 622、SB 619/B 619 SB 626/B 626、SB 366/B 366 、SB 462/B 462、SB 564/B 564、SB 462/B 462