Incoloy 25-6HN
Incoloy 25-6HNChemical composition:
C | Si | Mn | P | S | Ni | Cr | Mo | Cu | N |
≤0.030 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 23.5~ 25.5 |
20.0~ 22.0 |
6.0~ 7.0 |
≤0.75 | 0.18~ 0.25 |
Incoloy 25-6HNPhysical properties:
Density | 7.93g/cm | |
Melting point | 1360〜1394℃ | |
Specific heat | 451J/kg・K | |
Resistivity | 94.4μΩ・cm | |
Thermal conductivity | 11.9 | |
Average coefficient of thermal expansion | 20〜100℃ | 14.8 |
20〜200℃ | 15.3 | |
20〜300℃ | 15.6 | |
20〜400℃ | 15.9 | |
Magnetism | Not |
Incoloy 25-6HNMechanical properties:
size | Plate thickness(mm) | Yield strength(N/mm²) | Tensile strength(N/mm²) | Elongation(%) | hardness |
>4.8 ≤4.8 |
≥310 ≥310 |
≥650 ≥690 |
≥30 ≥30 |
≤240HBN ≤100HRB |
|
Hot rolled products | 6.0 | 422 | 770 | 49 | 207HBN |
Incoloy 25-6HNAlloy properties:
Excellent resistance to pitting and crevice corrosion in chloride solutions
Practical immunity to stress corrosion cracking in NaCl environments
High strength and toughness
Incoloy 25-6HNUses of alloys:
It is mainly used in FGD scrubbers, reverse osmosis, distillation columns, offshore oil and gas, and heat exchangers
Incoloy 25-6HNProcess performance:
Welding process: Laser welding or gas shielded welding with welding methods suitable for Incoloy 25-6HN, which often provide more uniform heating and cooling rates, helping to reduce crack formation.
Relevant standards:
ASTMB 688、ASTMA 240、ASTM B 675、ASTM A 312、ASTM B 676、ASTM A 249、ASTMB 804、ASTM B 691、ASTM A 479、ASTM B 462、ASTM A 182、ASTMB 564、ASTM B 366、ASTMB 472