Hastelloy G-3
Hastelloy G-3Chemical composition:
% | Ni | Fe | Cr | Mo | Cu | C | P | S | Mn | Si | Co | W | Nb |
Min | Bal | 18.0 | 21 | 6.00 | 1.5 | ≤ | |||||||
Max | 21.0 | 23.5 | 8.00 | 2.5 | 0.015 | 0.040 | 0.030 | 1.00 | 1.00 | 5 | 1.5 | 0.50 |
Hastelloy G-3Physical properties:
Density /g ·cm | Melting point/℃ | Thermal conductivity/W·(m·℃)-1 | Linear expansion coefficient/(10-6℃)-1 | Specific heat capacity/
J·(kg·℃)-1 |
Resistivity/
μΩ ·cm |
||||||
25℃ | 100℃ | 200℃ | 1007 | 200℃ | 300℃ | 25℃ | 100℃ | 200℃ | room temperature | ||
8.14 | 1260~ 1343 | 10.0 | 11.8 | 13.8 | 14.6 | 14.6 | 14.6 | 453 | 464 | 478 | 112.37 |
Hastelloy G-3Mechanical properties:
products | σb/MPa | oo.2/MPa | δ/% |
Thin and medium plates (solid solution) | 621 | 241 | 45 |
Oil & Gas Well Pipe Fittings (Cold Worked State) | 896 | 862 | 15 |
Hastelloy G-3Alloy properties:
High temperature resistance: Hastelloy G-3 alloy has excellent high temperature resistance. The material retains its physical and chemical stability in extreme high-temperature environments and is not prone to deformation or loss of performance.
Corrosion resistance: The alloy has good corrosion resistance, especially in environments containing chlorides, which makes it very suitable in industries such as chemical, oil, and gas.
Oxidation Resistance: Hastelloy G3 alloy has excellent oxidation resistance, which allows it to maintain its structural integrity at high temperatures.
Hastelloy G-3Uses of alloys:
This alloy is particularly suitable for equipment and components used in reductive corrosive environments such as phosphoric acid and sulfuric acid, as well as for components in FGD systems.
Hastelloy G-3Process performance:
Welding performance: G3 alloy has good weldability and can be welded by various methods common to welding high-nickel corrosion-resistant alloys. Solution treatment is generally not required after welding. In the case of SMAW welding, G3 electrode can be used, and in the case of GSAW welding, G3 wire can be used, and the corrosion resistance of the welded metal after welding is basically the same as that of the base metal.
Heat treatment process: Hastelloy G-3 can be heated at 1100~1150°C, and quickly cooled after heat preservation.
Relevant standards:
ASTM B 581、ASME SB-581、DIN 17752 、ASTM B 582、ASME SB-582、DIN 17750、ISO 6208 、ASTM B 619、ASME SB-619、ASTM B 775、ASME SB 775 、ASTM B 622、ASME SB-622、ASTM B 829、ASME SB 829、DIN 17751 、ASTM B 626、 ASME SB-626、ASTM B 751、ASME SB 751 、DIN 17744、ISO 9724、ASTM B 366、ASME SB 366