DD406
HuaNickel DD406 is a second-generation nickel-based single-crystal superalloy developed in China, which has the advantages of high temperature strength, good comprehensive performance, stable structure and good casting process performance. Compared with the second-generation single-crystal superalloys PWA1484, RenéN5 and CMSX-4 used abroad, its Tensile properties, durability, creep performance, oxidation resistance and hot corrosion resistance have reached or even partially exceeded its level, and it has the advantage of low cost because of its low Re content. The alloy has a durable strength of σ¹ ≥100 h, o ≥ 100 h, and is suitable for making high-temperature parts such as turbine working blades working below 1100°C and guide vanes working below 1150°C for gas turbines with complex inner cavities.
DD406 Chemical composition:
Ti | Cr | Co | W | Mo | AI | Nb | Ta | Re | Hf | Ti | Fe | B | Zr | Mn | Si | S | |
Min | Bal | 3.8 | 8.5 | 7 | 1.5 | 5.2 | 0.6 | 6 | 1.6 | 0.05 | ≤ | ||||||
Max | 4.8 | 9.5 | 9 | 2.5 | 6.2 | 1.2 | 8.5 | 2.4 | 0.15 | 0.1 | 0.2 | 0.02 | 0.1 | 0.15 | 0.2 | 0.001 |
DD406 Physical properties:
Density | 8.78g/cm³ |
Melting point | 1342℃~1399℃ |
Magnetic properties | not |
Coefficient of linear expansion
θ/℃ | 20~300 | 20~400 | 20~500 | 20~600 | 20~700 |
α/(10-6℃-I) | 11.92 | 12.59 | 12.93 | 13.15 | 13.53 |
θ/℃ | 20~800 | 20~900 | 20~1000 | 20~1100 | 20~1200 |
α/(10-6℃-I) | 14.19 | 14.39 | 15.00 | 15.76 | 16.75 |
Resilient performance
θ/℃ | 25 | 650 | 700 | 760 | 850 | 980 | 1070 | 1100 | |
E/GPa |
[001] | 131.5 | 107.5 | 107 | 105.5 | 98 | 80.5 | 69.5 | 67.5 |
[011] | 231.5 | — | 184.5 | 187.5 | 137.5 | 145 | 130 | 121 | |
[111] | 327 | — | 212 | 184.5 | 205 | 217.5 | 189 | 176.5 |
DD406 Mechanical properties:
Standard number | Variety | sampling | Long-lasting performance | Tensile properties | ||||||
θ/℃ | σ/MPa | τ/h | θ/℃ | σb/MPa | σp0.2/MPa | δ₅/% | ψ/% | |||
Q/6S 1678 |
Master alloy |
[001]Monocrystalline test sticksStandard heat treatment | 980 | 250 | ≥100 | 20 | ≥880 | ≥800 | ≥8 | ≥12 |
1070 | 140 | ≥100 | 760 | ≥1000 | ≥850 | ≥5 | ≥6 | |||
1100 | 130 | ≥100 | 980 | ≥700 | ≥600 | ≥18 | ≥22 |
DD406 Alloy properties:
DD406 is a second-generation nickel-based single-crystal superalloy, which has the advantages of high high temperature strength, good comprehensive performance, stable structure and good casting process performance.
DD406 Uses of alloys:
HuaNickel DD406 alloy has been selected for the fabrication of turbine working and guide vanes for a variety of advanced aero engines.
DD406 Process performance:
Parts Heat treatment: The blades with unprocessed surface should be treated with argon protection or vacuum, and then forced cooling by argon blowing, and the cooling rate should be greater than 260°C/min.
Relevant standards:
GB/T 14992 、Q/6S 1678