Alloy825

Loader Loading...
EAD Logo Taking too long?

Reload Reload document
| Open Open in new tab

Download [1.45 MB]

HuaNickel Alloy825 is a corrosion-resistant alloy Ni-Fe-Cr-Mo-Cu stabilized with titanium. This alloy has good comprehensive corrosion resistance and local corrosion resistance and good process properties, so it has been widely used in chemical, energy, petrochemical and hydrometallurgical industries.

Alloy825Chemical composition:

  Fe Ni Mo Cu Cr Ti C Si Mn P S AI
Min Bal 38 2.5 1.5 19.5 0.6
Max 46 3.5 3.5 23.5 1.2 0.05 0.5 1 0.04 0.03 0.2

Alloy825Physical properties:

Density/g·cm³ Melting point/℃ Coefficient of linear expansion/(10⁶ ·℃)-1 Thermalconductivity/W·(m·℃)-1 Resistivity/μΩ ·m Elastic modulusE/MPa×10³
20~100℃ 20~300℃ 25℃ 150℃ 20℃
8.14 1350 12.6 14.7 12.3 14.4 1.12 195

Alloy825Mechanical properties:

The state of heat treatment of the material Mechanical properties
σb/MPa σp0.2/MPa &;/% ψ/%%
Solution annealed tubes 608~647 264~323 44~53 ——

Alloy825Alloy properties:

The alloy has a pure austenite structure under solution conditions. However, at medium aging, carbides and intermetallic compounds can precipitate on austenite matrices and intergranular bodies, and these precipitated phases can impair the mechanical properties and corrosion resistance of the alloy.

Alloy825Uses of alloys:

Due to its wide range of corrosion resistance, this alloy is widely used in the chemical processing industry, hot seawater, and hydrometallurgical plants. It is mainly used to treat heat exchangers, pipes, valves, pumps, etc. in hot sulfuric acid, chloride-containing solution, sulfurous acid and other environments. It is also widely used in the field of wood pulp leachers and deep-source gas wells in the paper industry.

Alloy825Process performance:

Welding process: The usual welding method can be used, and nickel-based welding wire HuaNickel (00Cr22Ni61Mo9Nb) is recommended.

Heat Treatment: A suitable final heat treatment for this alloy is 940°C stable. The intermediate annealing temperature should be higher than 1050°C.

Relevant standards:

ASTM B 425,ASTM B 564,ASME SB 425,ASME SB 564,ASTM B 424, ASTM B 906, ASME SB 424, ASME SB 906, DIN 17750,, ISO 6208、ASTM B 163, ASTM B 423, ASTM B 704, ASTM B 705, ASTM B 751, ASTM B 775, ASTM B 829, ASME SB 163, ASME SB 423, ASME SB 704, ASME SB 705, ASME SB 751, ASME SB 775, ASME SB 829,ASTM B 366, ASME SB 366, DIN 17744

Detail datasheet