In a strong oxidizing environment, the corrosion resistance of Type HuaNickel 347 stainless steel is slightly improved compared to Type 321 stainless steel. Type HuaNickel 347 is stable with a column and is more suitable for aqueous and cryogenic environments due to its good resistance to intergranular attack. Both 347 and 321 are resistant to good polysulfuric acid stress corrosion cracking.

347Chemical composition:

  Fe Cr Ni Cb+Ta C Si Mn P S
Min Bal 17 9 Cb 10xc (Cb 8xC) 0.04
Max 19 13 1 0.08 0.75 2 0.45 0.03

347Physical properties:

Density Melting point
0.282 lb/in3 2550 – 2635°F

347Mechanical properties:

Temperature, °F 68 400 800 1000 1200 1350 1500
Ultimate tensile strength, ksi 93.3 73.6 69.5 63.5 52.3 39.3 26.4
0.2% yield strength, ksi 36.5 36.6 29.7 27.4 24.5 22.8 18.6

347Stainless steel characteristics:

Good creep strength up to 1500°F

Maintains good corrosion resistance in applications with temperatures between 800°F and 1500°F

Under welding conditions, it has good resistance to intergranular corrosion

347Uses of stainless steel:

Refineries, Fluid Catalytic Cracking Units (Face-Centered Cubes), Booms, Recovery Tube Sheet Housings, Brackets,

Relevant standards:

AMS: 5512 ASTM: A 240, A 262 Practice E ASME: SA-240

PWA: F17 LCS, PWA 300 MSRR:5632