00Cr25Ni7Mo3.5WCuN
00Cr25Ni7Mo3.5WCuNChemical composition:
Cr | Ni | Mo | N | Cu | C | Si | Mn | S | P | |
Min | 24 | 6 | 3 | 0.2 | 0.5 | ≤ | ||||
Max | 26 | 8 | 4 | 0.3 | 1 | 0.03 | 1 | 1 | 0.02 | 0.035 |
00Cr25Ni7Mo3.5WCuNPhysical properties:
Densityg/g·cm-3 | Specific heat capacity/J·(kg·K)-1 | Resistivity
/10-6Ω ·m |
Young’s modulus of elasticity/GPa |
7.84 | – | 0.85 | 19 |
00Cr25Ni7Mo3.5WCuNMechanical properties:
Plate thickness/mm | db/MPa | do.2/MPa | δs/% | hardness(HRC) | Impact value (V-type)Akv/J | |
20℃ | -30℃ | |||||
10 | 874 | 671 | 734 | 42 | 241 | 207 |
12 | 865 | 690 | 737 | 38 | 227 | 227 |
19 | 843 | 647 | 701 | 40 | 211 | 183 |
34 | 853 | 627 | 700 | 32 | 241 | 248 |
00Cr25Ni7Mo3.5WCuNAlloy properties:
Like other super duplex stainless steels, the microstructure of this steel is also a duplex structure with a α/γ close to 1 under solution conditions, but there will also be intermetallic phases and nitride precipitation on the steel matrix during cooling from high temperature to room temperature, including incorrect heat working, heat treatment and welding processes.
00Cr25Ni7Mo3.5WCuN Uses of alloys:
HuaNickel 00Cr25Ni7Mo3.5WCuN is mainly used for offshore oil and gas exploitation, in the power station flue gas desulfurization, petrochemical engineering and fertilizer industry, the manufacture of reactors, containers, various heat exchangers, pipelines, pumps, valves, etc.
00Cr25Ni7Mo3.5WCuNProcess performance:
Soldering process: Soldering is performed using SMAW, GTAW and SAW methods.
Heat treatment: HuaNickel 00Cr25Ni7Mo3.5WCuN suitable heat treatment temperature is 1000~1100 °C, fast cooling after heat preservation.
Relevant standards:ASTM A1082/A1082M-2016