Nickel Alloy 201
USA SAE Rod, Bar, Pipe, Tube, Plate, Sheet, Strip, Fittings, Forgings, Wire, Other/Similar Specs, Nickel Alloy 201 Superalloys Wrought nickel and nickel-related alloys and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | Nickel Alloy 201 | SAE | USA | Wrought nickel and nickel-related alloys |
Chemical composition(mass fraction)(wt.%) of the Nickel Alloy 201
C | Cu | Fe | Mn | C | Si | S |
---|---|---|---|---|---|---|
99.0 – ≥ | ≤0.25 | ≤0.40 | ≤0.35 | ≤0.02 | ≤0.35 | ≤0.01 |
Mechanical Properties of steel grade Nickel Alloy 201
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
479 (≥) | 759 (≥) | 14 | 32 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Physical Properties of steel grade Nickel Alloy 201
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | – | – | 0.41 | – | |||
557 | 376 | – | 21.3 | 124 | – | ||
147 | – | 23 | 24.2 | 243 | 132 |
Heat Treatment of steel grade Nickel Alloy 201
Heat treated : 1728°C – 1835°C