Technical Data Sheet
Chemical Composition Limits | |||||||
Weight% | C | Si | Mn | P+S max | Cr | Mo | Ni |
4S28 | 0.26-0.34 | 0.10-0.35 | 0.45-0.70 | P 0.025 S 0.020 |
1.10-1.40 | 0.20-0.35 | 3.90-4.30 |
Chemically similar British Specifications BS.970 Pt2 | |||||||
Weight% | C | Si | Mn | P+S max | Cr | Mo | Ni |
835M30 | 0.26-0.34 | 0.10-0.35 | 0.45-0.75 | P 0.025-0.050 S 0.025-0.040 |
1.10-1.40 | 0.20-0.35 | 3.90-4.30 |
EN30B | 0.26-0.34 | 0.10-0.35 | 0.40-0.60 | – | – | 0.20-0.40 | 3.90-4.30 |
Other Chemically similar Specifications | |||||||
Weight% | C | Si | Mn | P+S max | Cr | Mo | Ni |
AFNOR 30NCD16 | 0.25-0.35 | 0.10-0.40 | 0.20-0.55 | P 0.030 S 0.025 |
1.20-1.50 | 0.40-0.60 | 3.70-4.30 |
AFNOR 35NCD16 | 0.03-0.37 | 0.10-0.40 | 0.30-0.60 | P 0.030 S 0.025 |
1.60-2.00 | 0.30-0.50 | 3.70-4.20 |
WS 1.2766 NiCrMo16 |
0.32-0.38 | 0.15-0.30 | 0.40-0.60 | 0.035 max | 1.20-1.50 | 0.20-0.40 | 3.80-4.30 |
Typical Mechanical Properties
Grade | Treatment | Tensile Strength Rm (tonf/in²) | Proof Stress Rp 0.2, (tonf/in²) | Elongation in 5.65 √Cross Sectional Area % | Hardness HB | Ruling Section |
S28 | Solution Annealed | – | – | – | 285 max | 2 1/2" |
S28 | Hardened and Tempered | 100 | 73 | 8 | 444 | 2 1/2" |
Availability
Alloy S28 is available in Bar. For all stock availability contact Sales.