Chemical composition(mass fraction)(wt.%) of the Y1Cr13
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
Max 0.15 | Max 1.00 | Max 1.25 | 0.06 | Max 0.15 | 12.00-14.00 | Max 0.60 | Max 0.60 |
Mechanical Properties of steel grade Y1Cr13
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
789 (≥) | 637 (≥) | 24 | 43 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Physical Properties of steel grade Y1Cr13
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | – | – | 0.14 | – | |||
577 | 759 | – | 43.3 | 421 | – | ||
272 | – | 22 | 23.2 | 423 | 324 |
Heat Treatment of steel grade Y1Cr13
Heat treated : 1479°C – 1983°C
Technological Curves of steel grade Y1Cr13