Chemical composition(mass fraction)(wt.%) of the H26

C Si Mn P S Cr Mo V W Ni+Cu
0.45 -0.55 0.15 -0.40 0.15 -0.40 ≤0.030 ≤0.030 3.75 -4.50 ≤ ≥ 0.75 -1.25 17.25 -19.00 ≤0.75



Mechanical Properties of steel grade H26

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
987 (≥) 913 (≥) 24 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical Properties of steel grade H26

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
21     0.21  
834 122 41.3 144    
568 34 14.2   424 324

Heat Treatment of steel grade H26

Heat treated : 1612°C – 1849°C

Technological Curves of steel grade H26