USA UNS T20826 Tool Die Steels Hot-Work Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Category Class Grade Standard Country Application
Steel Grades Tool Die Steels T20826 UNS USA Hot-Work Tool Steel


Chemical composition(mass fraction)(wt.%) of the T20826

C Si Mn P S Cr Mo V W Ni+Cu
0.45 -0.55 0.15 -0.40 0.15 -0.40 ≤0.030 ≤0.030 3.75 -4.50 ≤ ≥ 0.75 -1.25 17.25 -19.00 ≤0.75



Mechanical Properties of steel grade T20826

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
172 (≥) 491 (≥) 24 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical Properties of steel grade T20826

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32     0.33  
129 732 42.3 222    
449 12 24.2   241 313

Heat Treatment of steel grade T20826

Heat treated : 1664°C – 1195°C

Technological Curves of steel grade T20826

Cross Reference Table (Equivalent Grade) of T20826

Grade Standard Country Application
UNS T20826
T20826